EP30P Two part, room temperature curing epoxy system with excellent optical transparency. Low viscosity. Bonds extremely well to more sensitive plastics such as polycarbonates and acrylics. Superior electrical insulation properties. Good chemical resistance to oils, fuels, water, hydraulic fluids. Serviceable from -60°F to +250°F. |
|
EP42HT-2FG Black Food grade epoxy system certified to meet FDA CFR 175.105. Excellent resistance to fats, oils, acids, alkalis and many solvents. Withstands boiling water, radiation, chemicals, steam and frozen storage conditions. Strong bonds to similar/dissimilar substrates. Service temperature range -60°F to +450°F. Black in color. |
|
EP42HT-2FG Food grade epoxy system toxicologically evaluated to meet the NSF/ANSI 51.4.1 (2009) standard for food equipment materials. Certified to meet FDA CFR 175.300. Excellent resistance to fats, oils, acids, alkalis and many solvents. Withstands boiling water, radiation, chemicals, steam and frozen storage conditions. Strong bonds to similar/dissimilar substrates. Service temperature range -60°F to +450°F. Low viscosity. |