EP51FL-1ND-2 Flexible epoxy adhesive has rapid set up time and cure speed. High peel strength and elongation. Withstands mechanical shock and vibration. Resists thermal cycling. Superb electrical insulation properties. Service operating temperature range from -100°F to +250°F. |
|
EP51HT Service operating temperature range from 4K to +400°F. Fast room temperature curing epoxy adhesive/sealant. Gels in 5 minutes. Convenient one to one mixing ratio by weight. Bonds well to similar/dissimilar substrates. High tensile lap shear strength. |
|
EP51ND High viscosity paste. Does not drip on vertical surfaces. Fast "5 minute" curing, two component epoxy adhesive. High bond strength. Serviceable from -100°F to +250°F. Superior durability. One to one mix ratio weight or volume. Excellent dielectric properties. |
|
EP52TC Low thermal resistance properties. Can be applied in bond lines as thin as 10-15 microns. Low CTE. Low shrinkage upon cure. Serviceable from -100°F to +300°F. Exceptional dimensional stability. |
|
EP53TC Low thermal resistance properties. Can be applied in bond lines as thin as 10-15 microns. Low CTE. Low shrinkage upon cure. Serviceable from -100°F to +300°F. Exceptional dimensional stability. |
|
EP54TC Very high thermal conductivity over 6 W/(m•K). Combines very high thermal conductivity and robust electrical insulation. Used for bonding and sealing. Paste consistency with long working life. |
|
EP62-1 Cures rapidly at moderate elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Withstands aggressive chemical exposure. Tg 160-165°C. Shore D hardnes >80. |
|
EP62-1AO Cures rapidly at moderate elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Withstands aggressive chemical exposure. Tg 160-165°C. Shore D hardnes >80. |
|
EP62-1BF Cures rapidly at moderate elevated temperatures. Superior resistance to harsh chemicals. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +500°F. Tg 170-175°C. Shore D hardness 80-90. |
|
EP62-1HT Superior resistance to harsh chemicals, particularly to acids. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Ideal for bonding and coating. Good flow. Reliable electrical insulator. Serviceable from -60°F to +450°F. Tg 150-160°C. Shore D hardness 80-90. |