357 products match
|
EP42HT-2Med Black USP Class VI approved. Serviceable from -60°F to 450°F. Withstands multiple cycles of medical sterilization including radiation, EtO, autoclaving and chemical sterilants. Shore D hardnes >75. Used for bonding, sealing, coating, casting. Can be cured up to 2-3 inches thick. Cures at ambient temperature or more quickly at elevated temperatures. |
|
EP42HT-2Med Low viscosity, two part epoxy with outstanding chemical resistance. Passes USP Class VI biocompatibility tests. Capable of withstanding repeated sterilization cycles including radiation, EtO, chemical sterilants, autoclaving. Serviceable from -60°F to +450°F. Cures at room or elevated temperatures. Available in amber-clear and black colors. Castable in thicknesses up to 2-3 inches. |
|
EP42HT-2ND-2 Serviceable from -60°F to 450°F. Cures at ambient temperatures, or faster with heat. Tensile strength 10,000-11,000 psi. Shore D hardness 80-90. Superior dimensional stability. Remarkable chemical resistance. |
|
EP42HT-2ND-2Med Black Two component epoxy paste adhesive. Resists sterilization exposure. USP Class VI approved. Outstanding thermal stability and electrical insulation properties. Cures at ambient temperatures. Withstands multiple cycles of autoclaving, radiation, EtO and chemical sterilants. Post curing is recommended to optimize physical properties. Serviceable from -60°F to +450°F. |
|
EP42HT-3AO Thermally conductive, electrically insulative. Ideal for potting and encapsulation. Castable up to 3-4 inches. Excellent chemical resistance. Enhanced thermal cycling capabilities. Good flow. Serviceable from -100°F to +400°F. Impervious to intermittent exposures to steam. Shore D hardnes >80. |
|
EP42HT-4AOMed Black Thermally conductive, electrically insulative two part epoxy. Meets USP Class VI and ISO 10993-5 certifications. Cryogenically serviceable from 4K to +400F. NASA low outgassing aproved. Black in color. For bonding, sealing, coating and casting. |
|
EP45AOHT Thermally conductive/eletrically insulative epoxy serviceable from -60°F to +500°F. Heat curing. Paste viscosity. Superior chemical resistance properties. Gap filling. Long pot life. Withstands thermal cycling. Gray color. |
|
EP45HT High performance adhesive/sealant/coating. Serviceable from -80°F to +500°F. Resists thermal cycling. Outstanding resistance to acids, bases, petrochemicals, water. 100% reactive. Cures at elevated temperatures. Good flow properties. Moderate viscosity. Excellent performance profile for long term exposures at 400°F to 450°F. Well suited for moderate sized electronic potting applications. |
|
EP45HTAN Thermally conductive/eletrically insulative epoxy serviceable from 4K to +500°F. Heat curing. Excellent strength retention at high temperatures. High dimensional stability and low shrinkage upon cure. Superior chemical resistance properties. |
|
EP45HTMed USP Class VI certified. Withstands repeated cycles of sterilization such as autoclaving, radiation and chemical sterilants. High bond strength. Heat curing. Two component epoxy system. Long pot life. Service operating temperature range from -80°F to +500°F. |