Visible light curable adhesives feature high bond strength, thermal stability, chemical and water resistance and excellent surface cure. These one component compounds are designed to provide safe and rapid cures upon exposure to LED light at ambient temperatures. Environmentally friendly, these formulations are solvent free and contain no volatiles.

Master Bond Products Covered in this Infographic
|
LED401 One part, no mix, fast curing compound. Tack free cure. High bond strength to a wide range of substrates. Solvent free formulation. Withstands 1,000 hours 85°C/85% RH. Serviceable from -60°F to +250°F. |
|
LED401LV One part, low viscosity, optically clear system. Fast curing with a high bond strength. Superior dimensional stability and electrical insulative properties. Serviceable from -60°F to +250°F. |
|
LED401 White High viscosity, one component system in white. Excellent dimensional stability, electrical insulation properties and good chemical resistance upon cure. Serviceable from -60°F to +250°F. |