Master Bond Products Covered in this Infographic
|
MasterSil 705TC Thermally conductive and electrically isolating. Easy to use silicone for high performance bonding, sealing and coating. Non-corrosive and room temperature curable. Ideally suited for applications requiring flexibility and high temperature resistance. |
|
MasterSil 711 Exceptionally fast setting, high performance, non-corrosive silicone rubber. Widely used in manufacturing and repair applications. Has superb flexibility. Servicable from -75°F to +400°F. |
|
MasterSil 800 Ultra high temperature resistance up to 300°C. Superb flexibility and elasticity. Non-corrosive. One component, room temperature curing. Flowable. |